高速铁路桥梁桥面二次防水层施工质量控制(51 卷) |
英文标题 |
Construction quality control of second waterproofing on surface of girder of high speed railway bridge |
摘要 |
桥面防水是CRTS Ⅱ无砟轨道的重要工序,且桥面二次防水施工的质量控制难度较大。本文介绍了桥面防水的主要施工工艺,并全面分析了质量控制重点、难点及对策。实践表明,必须从原材料、基面处理、底涂、特殊部位处理、施工环境及工序时间选择、施工成品保护等方面进行全面控制 |